- 描述
- 询问
描述
CHY-03 负载软蠕变试验机
介绍
This instrument is used to detect the resistance of refractory materials under the action of high temperature load softening, and is an important index for detecting the high temperature mechanical properties of refractory materials. Meet the national standard GB/T5073-2005 “Refractories compression creep test method” and GB/T5989-2008 and ISO3187-1989 “Refractories load softening temperature test method”, with computer automatic testing, 数据处理, automatically generate temperature and deformation curves and save.
主要技术参数:
Normal operating temperature (℃) Load soft 1700℃, creep: 1550℃
2, 加热速度: 0 ~ 10℃/min
3, 温度控制精度: ±1℃
4, temperature uniformity: ±10℃
5, deformation measurement range: 0 ~ 10mm
6, deformation measurement accuracy: 0.1%
7, loading range: 0.05 ~ 0.2MPa
8. Number of continuous samples :3.
9, heating element: silicon molybdenum rod;
10, 热电偶: B index number.
11, 连接电脑自动测试, 数据处理, and can produce the test report print out.