Descriere

GA-1903 Analizator de scanare diferențială DSC

Introducerea Produsului:

GA-1903 is the company launched DSC series of products with the highest accuracy of one, the sensor is the use of imported material E-couple, precizie ridicata, sensibilitate ridicată, good repeatability, signal acquisition circuit shielding protection, puternic anti-interferență, baseline stability and repeatability is very high.

GA-1903 differential scanning calorimeter, can be glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature and product stability, oxidation induction period and other tests. It is qualified for the research of pipe, polymer, chimic, alimente, medicale și alte domenii, and serves universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.

GA-1903 Analizator de scanare diferențială DSC

Technical Features:

  1. Industrial grade 7 inch touch screen, display rich information
  2. New furnace body structure, better baseline, higher accuracy. Heating adopts indirect conduction mode, high uniformity and stability, reduce pulse radiation, better than the traditional heating mode.
  3. 3.Interfață de comunicare USB, strong commonality, reliable communication without interruption, support self-recovery connection function.
  4. Automatic switching of two air flow, fast switching speed, short stability time. În același timp, a protective gas input is added.
  5. Software is simple and easy to operate.
  6. Ultra-high sensitivity, precizie, 0.001 MW, 0.001℃
  7. Exquisite technical indicators, superior performance, cost-effective, widely used

GA-1903 Analizator de scanare diferențială DSC

Tparametrii tehnici:

  1. Interval de temperatură: room temperature ~550℃
  2. temperature resolution: 0.001℃
  3. temperature fluctuation :±0.001℃
  4. Repetabilitatea temperaturii :±0.01℃
  5. Rata de încălzire: 0.1 ~ 80℃/min
  6. Constant temperature time: program setting ≤24h
  7. Temperature control mode: heating, constant temperature, cooling (automatic program control)
  8. DSC range: 0 ~ ±600mW
  9. DSC resolution: 0.01uW
  10. DSC sensitivity: 0.001mW
  11. Alimentare electrică: AC220V/50Hz or customized
  12. Atmosphere control gas: nitrogen, oxygen (program setting/automatic switch)
  13. Gas flow: 0-300ml /min
  14. gas pressure: 0.2MPA
  15. Modul de afișare: 24Culoare, 7 Ecran tactil LCD inch LCD
  16. Interfață de date: standard USB interface
  17. Standardul parametrilor: equipped with standard material (indium, staniu), users can adjust the temperature by themselves
  18. The instrument has multiple groups of thermocouples, one group to measure sample temperature, one group to measure furnace body temperature, and one group to measure internal environment temperature
  19. Cooling device: air cooling device (optional semiconductor & LT; – 40 ~ 550 ℃ & gt; Liquid nitrogen refrigeration < – 150 ~ 550 ℃ & gt;)