CHY-03 Load Soft Creep Tester

Wstęp

This instrument is used to detect the resistance of refractory materials under the action of high temperature load softening, and is an important index for detecting the high temperature mechanical properties of refractory materials. Meet the national standard GB/T5073-2005 “Refractories compression creep test method” and GB/T5989-2008 and ISO3187-1989 “Refractories load softening temperature test method”, with computer automatic testing, data processing, automatically generate temperature and deformation curves and save.

CHY-03 Load Soft Creep Tester

Główne parametry techniczne:

Normal operating temperature (℃) Load soft 1700℃, creep: 1550℃

2, heating speed: 0 ~ 10℃/min

3, Dokładność kontroli temperatury: ±1 ℃

4, równomierność temperatury: ±10℃

5, deformation measurement range: 0 ~ 10mm

6, deformation measurement accuracy: 0.1%

7, loading range: 0.05 ~ 0.2MPa

8. Number of continuous samples :3.

9, heating element: silicon molybdenum rod;

10, thermocouple: B index number.

11, connect the computer automatic test, data processing, and can produce the test report print out.