CHY-03 Muatkan Penguji Rayapan Lembut

pengenalan

This instrument is used to detect the resistance of refractory materials under the action of high temperature load softening, dan merupakan indeks penting untuk mengesan sifat mekanikal suhu tinggi bahan refraktori. Memenuhi standard kebangsaan GB/T5073-2005 “Kaedah ujian rayapan mampatan refraktori” and GB/T5989-2008 and ISO3187-1989 “Refractories load softening temperature test method”, with computer automatic testing, data processing, automatically generate temperature and deformation curves and save.

CHY-03 Muatkan Penguji Rayapan Lembut

Parameter teknikal utama:

Normal operating temperature (℃) Load soft 1700℃, merayap: 1550℃

2, heating speed: 0 ~ 10℃/min

3, temperature control accuracy: ±1 ℃

4, keseragaman suhu: ±10℃

5, deformation measurement range: 0 ~ 10mm

6, deformation measurement accuracy: 0.1%

7, loading range: 0.05 ~ 0.2MPa

8. Number of continuous samples :3.

9, heating element: silicon molybdenum rod;

10, thermocouple: B index number.

11, connect the computer automatic test, data processing, and can produce the test report print out.