Keterangan

GA-1908 Differential Scanning Calorimeter

perkenalan produk:

The differential scanning calorimeter is touch-screen and can be used for glass transition temperature measurement, phase transition measurement, melting and enthalpy measurement

Value test, product stability, oxidation induction period test, specific heat test, dll.. Mainly used in chemical, energi, metalurgi, mineral, polymer materials, metal materials and other industries

GA-1908 Differential Scanning Calorimeter

Parameter teknik:

  1. Kisaran suhu: -170~600℃, liquid nitrogen refrigeration
  2. Temperature resolution: 0.01℃
  3. Fluktuasi suhu: ±0.01℃
  4. Temperature repeatability: ±0.1℃
  5. Tingkat pemanasan: 0.1 ~ 80℃/min
  6. Constant temperature time: 0~ 400
  7. Temperature control mode: heating, pendinginan, constant temperature
  8. DSC range: 0 ~ ±600mW
  9. DSC resolution: 0.001mW
  10. DSC sensitivity: 0.001mW
  11. Sumber Daya listrik: AC220V/50Hz or customized
  12. Cooling equipment: liquid nitrogen cooling
  13. Atmosphere control gas: nitrogen, oxygen (automatic instrument switch)
  14. Gas flow: 0-300ml /min
  15. gas pressure: 0.2mpa
  16. Mode tampilan: 24bit color, 7 inch LCD touch screen display
  17. Data interface: standard USB interface
  18. Parameter standard: equipped with standard material (indium, timah), users can adjust the temperature
  19. Upper computer operation software, coordinate range automatically switch, no manual adjustment; Software analysis results can be dragged at will display position
  20. The instrument has multiple groups of thermocouples, one group to test the sample temperature, one group to test the internal environment temperature of the instrument, and one group to test the furnace temperature

GA-1908 Differential Scanning Calorimeter

Technical features:

  1. Industrial grade 7 Layar sentuh inci, display rich information.
  2. New furnace body structure, can be matched with a variety of refrigeration devices.
  3. USB communication interface, strong commonality, reliable communication without interruption, support self-recovery connection function.
  4. Automatic switching of two air flow, fast switching speed, short stability time. Pada saat yang sama, a protective gas input is added.
  5. Software is simple and easy to operate.