Popis

GA-1903 DSC diferenciální skenovací analyzátor

Představení produktu:

GA-1903 is the company launched DSC series of products with the highest accuracy of one, the sensor is the use of imported material E-couple, vysoká přesnost, vysoká citlivost, good repeatability, signal acquisition circuit shielding protection, silná ochrana proti rušení, baseline stability and repeatability is very high.

GA-1903 differential scanning calorimeter, can be glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature and product stability, oxidation induction period and other tests. It is qualified for the research of pipe, polymer, chemical, jídlo, medical and other fields, and serves universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.

GA-1903 DSC diferenciální skenovací analyzátor

Technický Features:

  1. Industrial grade 7 inch touch screen, zobrazovat bohaté informace
  2. New furnace body structure, better baseline, higher accuracy. Heating adopts indirect conduction mode, high uniformity and stability, reduce pulse radiation, better than the traditional heating mode.
  3. 3.USB communication interface, strong commonality, reliable communication without interruption, support self-recovery connection function.
  4. Automatic switching of two air flow, fast switching speed, short stability time. Ve stejnou dobu, a protective gas input is added.
  5. Software is simple and easy to operate.
  6. Ultra-high sensitivity, přesnost, 0.001 MW, 0.001℃
  7. Exquisite technical indicators, superior performance, nákladově efektivní, widely used

GA-1903 DSC diferenciální skenovací analyzátor

Ttechnické parametry:

  1. Teplotní rozsah: room temperature ~550℃
  2. temperature resolution: 0.001℃
  3. temperature fluctuation :±0.001℃
  4. Temperature repeatability :±0.01℃
  5. Rychlost ohřevu: 0.1 ~ 80℃/min
  6. Doba konstantní teploty: program setting ≤24h
  7. Temperature control mode: heating, constant temperature, cooling (automatic program control)
  8. DSC range: 0 ~ ±600mW
  9. DSC resolution: 0.01uW
  10. DSC sensitivity: 0.001mW
  11. Zdroj napájení: AC220V/50Hz or customized
  12. Atmosphere control gas: nitrogen, oxygen (program setting/automatic switch)
  13. Gas flow: 0-300ml /min
  14. gas pressure: 0.2mpa
  15. Režim zobrazení: 24bit color, 7 inch LCD touch screen display
  16. Data interface: standard USB interface
  17. Parameter standard: equipped with standard material (indium, cín), users can adjust the temperature by themselves
  18. The instrument has multiple groups of thermocouples, one group to measure sample temperature, one group to measure furnace body temperature, and one group to measure internal environment temperature
  19. Chladící zařízení: air cooling device (optional semiconductor & LT; – 40 ~ 550 ℃ & gt; Liquid nitrogen refrigeration < – 150 ~ 550 ℃ & gt;)